We used a hammer a piece of felt a rock and safety goggles when breaking up the glass.
How to melt glass into flat sheets.
Glass separator recommended or kiln wash adequate can be purchased in powder form and mixed to a liquid.
Crushed pieces can be placed inside a mold by frit casting at 1480 f.
There are still many things to learn and know when you melt glass at home and create glass art.
Glass marbles can be melted until they stick together using the tack fusing method at 1350 f.
Place a plexiglass sheet on large pan and place on the middle oven rack.
Then continue to raise your kiln s temperature and watch the glass until the glass reaches the consistency you want usually around 1500 degrees fahrenheit.
Bottles can be melted by draping which is letting the weight of melted glass shape over a mold at 1200 f.
Preheat the oven to 250 degrees f.
Annealing is where you allow your glass to rest at a temperature below its freezing point which is a little below 1000 f 537 c for many kinds of glass.
Make the surface as even as possible since tiny irregularities will show up in the glass.
Lakeside pottery writes that standard soda lime silica the most common kind of natural glass melts at 1500 c around 2700 f while pure silica needs fluxes to melt at a lower temperature it s best to fire the work slowly to start with.
As with clay glass changes state at varying temperatures according to the components it s made from.
Fold the felt in half with the glass in the middle.
The large pan prevents the plexiglass from coming into contact with the hot rack which can distort the plexiglass due to uneven heating.
Small pieces are easiest to arrange and to get into all the little corners.
Place the felt on top of the rock and while wearing safety goggles use the hammer to break the glass.
Brush it on in at least four coats then wait for it to dry.
Leave the temperature at 1000 degrees for 15 minutes to allow all the glass pieces to reach the same temperature.
There have been four phases of making flat glass pouring the glass out and rolling it cast glass blowing a cylinder and cutting the side while it is hot then flattening blowing a rondel disk cut into panes and blowing a cylinder then cooling to break off ends and length then sagging it flat.
Heat for approximately five minutes.